RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of GaSe (Gallium selenide)
Kato et al. 2013: n(o) 0.8-1620 µm

Wavelength: µm
 (0.8 – 1620)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=10.6409+\frac{0.3788}{λ^2-0.1232}+\frac{7090.7}{λ^2-2216.3}$$

Comments

20 °C, Ordinary ray (o)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

K. Kato et al.. Sellmeier and thermo-optic dispersion formulas for GaSe (Revisited). Appl. Opt. 52, 2325-2328 (2013)

More info - wiki

Gallium selenide, GaSe