Optical constants of Cu (Copper)
Brimhall et al. 2009: n,k 0.0101-0.0421 µm

Wavelength: µm
 (0.0101 – 0.0421)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

N. Brimhall, N. Herrick, D. D. Allred, R. S. Turley, M. Ware, J. Peatross. Measured optical constants of copper from 10 nm to 35 nm, Optics Express 17, 23873-23879 (2009)