Optical constants of Cu (Copper)
Babar and Weaver 2015: n,k 0.2066-12.40 µm

Wavelength: µm
 (0.2066 – 12.40)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

S. Babar and J. H. Weaver. Optical constants of Cu, Ag, and Au revisited, Appl. Opt. 54, 477-481 (2015)