Optical constants of CsI (Cesium iodide)
Rodney 1955: 0.2967-50 µm; 24 °C

Wavelength: µm
 (0.2967 – 50)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.34617251λ^2}{λ^2-0.0229567^2}+\frac{1.0080886λ^2}{λ^2-0.1466^2}+\frac{0.28551800λ^2}{λ^2-0.1810^2}+\frac{0.39743178λ^2}{λ^2-0.2120^2}+\frac{3.3605359λ^2}{λ^2-161.0^2}$$

Comments

24 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

W. S. Rodney. Optical properties of cesium iodide, J. Opt. Soc. Am. 45, 987-991 (1955)