Optical constants of Chromium (Cr)
Johnson and Christy 1974: n,k 0.188-1.937 µm

Wavelength: µm
 (0.188 – 1.937)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Room temperature

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

P. B. Johnson and R. W. Christy. Optical constants of transition metals: Ti, V, Cr, Mn, Fe, Co, Ni, and Pd, Phys. Rev. B 9, 5056-5070 (1974)

More info - wiki

Chromium, Cr

External links