Optical constants of CdSe (Cadmium selenide)
Lisitsa et al. 1969: n(o) 1.01-22.0 µm

Wavelength: µm
 (1.01 – 22)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=3.2243+\frac{1.7680λ^2}{λ^2-0.2270}+\frac{3.1200λ^2}{λ^2-3380}$$

Comments

Ordinart ray (o)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) M. P. Lisitsa et al.. Dispersion of the refractive indices and birefringence of CdSxSe1-x single crystals, Phys. Status Solidi, 31, 389-399 (1969)
2) G. C. Bhar, Refractive index interpolation in phase-matching, Appl. Opt. 15, 305-307 (1976)
*Ref. 2 provides Sellmeier equation based on the data from Ref. 1