RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of CaMoO4 (Calcium molybdate)
Bond 1965: n(o) 0.45-3.8 µm

Wavelength: µm
 (0.45 – 3.8)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{2.7840λ^2}{λ^2-0.1483^2}+\frac{1.2425λ^2}{λ^2-11.576^2}$$

Comments

Ordinary ray (o). Room temperature.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) W. L. Bond. Measurement of the refractive indices of several crystals , J. Appl. Phys. 36, 1674-1677 (1965)
2) Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009
* Ref. 2 provides Sellmeier equation based on the data from ref. 1

More info - wiki

Calcium molybdate, CaMoO4

Mineral name

Powellite