Optical constants of C (Carbon)
Phillip and Taft 1964: Diamond; n,k 0.0354-10 µm

Wavelength: µm
 (0.035424054 – 10.00000000)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. R. Phillip and E. A. Taft. Kramers-Kronig Analysis of Reflectance Data for Diamond, Phys. Rev. 136, A1445-A1448 (1964)