Optical constants of C (Carbon)
Larruquert et al. 2013: Tetrahedral amorphous thin film; n,k 0.01966-10.07 µm

Wavelength: µm
 (0.019656426 – 10.07918931)  
 

Other optical constants

n   k   logX   logY   eV

Comments

ta-C: tetrahedral amorphous carbon. Density: 3.25 g/cm3.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

J. I. Larruquert, L. V. Rodríguez-de Marcos, J. A. Méndez, P. J. Martin, A. Bendavid. High reflectance ta-C coatings in the extreme ultraviolet, Opt. Exp. 21, 27537-27549 (2013) (Numerical data kindly provided by Juan Larruquert)