RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of C (Carbon)
Djurišić and Li 1999: Graphite; n,k (e); 0.0310-0.5904 µm

Wavelength: µm
 (3.0996e-02 – 5.9040e-01)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Graphite. Extraordinary ray (e). Critical analysis and fit of the experimental data from several sources to a modified Lorentz-Drude (LD) model.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: true
λ_is_vacuum: true

References

A. B. Djurišić and E. H. Li. Optical properties of graphite, J. Appl. Phys. 85, 7404-7410 (1999)
[Calculation script (Python)]

More info - wiki

Carbon, C

Most common allotropes

Diamond (cubic carbon); Graphite; Amorphous carbon; Graphene