Optical constants of BiB3O6 (Bismuth triborate, BiBO)
Umemura et al. 2007: n(α) 0.48-3.1 µm

Wavelength: µm
 (0.48 – 3.1)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=3.07403+\frac{0.03231}{λ^2-0.03163}-0.013376λ^{2}$$

Comments

nα; 20 °C.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

N. Umemura, K. Miyata, and K. Kato. New data on the optical properties of BiB3O6, Opt. Mat. 30, 532-534 (2007)

More info - wiki

Bismuth triborate, BiB3O6 (BiBO)

Other name

Bismuth borate, BIBO