RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of BaB2O4 (Barium borate, BBO)
Zhang et al. 2000: BBO; n(o) 0.64-3.18 µm

Wavelength: µm
 (0.64 – 3.18)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=2.7359+\frac{0.01878}{λ^2-0.01822}-0.01471λ^{2}+0.0006081λ^{4}-0.00006740λ^{6}$$

Comments

Beta barium borate (ß-BaB2O4, BBO). Ordinary ray (o). Near infrared.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. Zhang, Y. Kong, J.-Y. Zhang. Optical parametric properties of 532-nm-pumped beta-barium-borate near the infrared absorption edge, Optics Communications, 184, 485-491 (2000)

More info - wiki

Barium borate, BaB2O4 (BBO)

Most common allotrope

Beta barium borate (ß-BaB2O4)

External links