Optical constants of Au (Gold)
Windt et al. 1988: n,k 0.0024-0.1216 µm

Wavelength: µm
 (0.00236 – 0.12157)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. L. Windt, W. C. Cash, M. Scott, P. Arendt, B. Newnam, R. F. Fisher, A. B. Swartzlander. Optical constants for thin films of Ti, Zr, Nb, Mo, Ru, Rh, Pd, Ag, Hf, Ta, W, Re, Ir, Os, Pt, and Au from 24 Å to 1216 Å, Appl. Opt. 27, 246-278 (1988)