Optical constants of Au (Gold)
Olmon et al. 2012: Single-crystal gold; n,k 0.300-24.93 µm

Wavelength: µm
 (3.000E-01 – 2.493E+01)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Single-crystal gold

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

R. L. Olmon, B. Slovick, T. W. Johnson, D. Shelton, S.-H. Oh, G. D. Boreman, and M. B. Raschke. Optical dielectric function of gold, Phys Rev. B 86, 235147 (2012) (see Supplemental Material for numerical data)