RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Au (Gold)
Johnson and Christy 1972: n,k 0.188-1.937 µm

Wavelength: µm
 (0.1879 – 1.9370)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Room temperature

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

P. B. Johnson and R. W. Christy. Optical Constants of the Noble Metals, Phys. Rev. B 6, 4370-4379 (1972)

More info - wiki

Gold, Au

External links