Optical constants of Au (Gold)
Hagemann et al. 1974 #2: n,k 0.003542-0.8266 µm

Wavelength: µm
 (3.542E-03 – 8.266E-01)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) H.-J. Hagemann, W. Gudat, and C. Kunz. Optical constants from the far infrared to the x-ray region: Mg, Al, Cu, Ag, Au, Bi, C, and Al2O3, J. Opt. Soc. Am. 65, 742-744 (1975)
2) H.-J. Hagemann, W. Gudat, and C. Kunz. DESY report SR-74/7 (1974)

More info - wiki