Optical constants of Ar (Argon)
Sinnock and Smith 1969: Liquid at 90 K; n 0.3612-0.6439 µm

Wavelength: µm
 (0.3612 – 0.6439)  
 

Other optical constants

logX   logY   eV

Comments

Liquid argon at 90 K (-183.15 °C).

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

temperature: 90 K

References

A. C. Sinnock and B. L. Smith. Refractive indices of the condensed inert gases, Phys. Rev. 181, 1297-1307 (1969)