Optical constants of Al (Aluminium)
Rakić 1995: 0.00012399-200 µm

Wavelength: µm
 (1.2399E-04 – 2.0000E+02)  
 

Other optical constants

n   k   logX   logY   eV

Comments

"Optical and electron-energy-loss data for evaporated-aluminum films have been critically analyzed and used in an iterative, self-consistent algorithm that represents a combination of the Kramers-Kronig analysis and the semiquantum-model application."

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. D. Rakić. Algorithm for the determination of intrinsic optical constants of metal films: application to aluminum, Appl. Opt. 34, 4755-4767 (1995)