RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Al (Aluminium)
Ordal et al. 1988: n,k 0.667-200 µm

Wavelength: µm
 (0.667 – 200)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. A. Ordal, R. J. Bell, R. W. Alexander, L. A. Newquist, M. R. Querry. Optical properties of Al, Fe, Ti, Ta, W, and Mo at submillimeter wavelengths, Appl. Opt. 27, 1203-1209 (1988)

More info - wiki

Aluminium, Al

Other name

Aluminum

External links