RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Al (Aluminium)
Hagemann et al. 1974: n,k 0.00001033-1240 µm

Wavelength: µm
 (1.033E-05 – 1.240E+03)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) H.-J. Hagemann, W. Gudat, and C. Kunz. Optical constants from the far infrared to the x-ray region: Mg, Al, Cu, Ag, Au, Bi, C, and Al2O3, J. Opt. Soc. Am. 65, 742-744 (1975)
2) H.-J. Hagemann, W. Gudat, and C. Kunz. DESY report SR-74/7 (1974)

More info - wiki

Aluminium, Al

Other name

Aluminum

External links