Optical constants of AgGaSe2 (Silver gallium selenide, AGSe)
Boyd et al. 1972: n(o) 0.725-13.5 µm

Wavelength: µm
 (0.725 – 13.5)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=3.6453+\frac{2.2057λ^2}{λ^2-0.1879}+\frac{1.8377λ^2}{λ^2-1600}$$

Comments

Ordinary ray (e)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) G. D. Boyd et al.. Linear and nonlinear optical properties of some ternary selenides, IEEE J. Quant. Electron., 8, 900-908 (1972)
2) G. C. Bhar, Refractive index interpolation in phase-matching, Appl. Opt. 15, 305-307 (1976)
*Ref. 2 provides Sellmeier equation based on the data from Ref. 1