Optical constants of AgBr (Silver bromide)
Schröter 1931: n 0.495-0.67 µm

Wavelength: µm
 (0.495 – 0.67)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$\frac{n^2-1}{n^2+2}=0.452505+\frac{0.09939λ^2}{λ^2-0.070537}-0.000150λ^2$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. Schröter. Über die Brechungsindizes einiger Schwermetallhalogenide im Sichtbaren und die Berechnung von Interpolationsformeln für den Dispersionsverlauf (On the refractive indices of some heavy-metal halides in the visible and calculation of interpolation formulas for dispersion), Z. Phys. 67, 24-36 (1931) [in German]