Optical constants of Soda lime glass
Rubin 1985: Grey; n,k 0.32-4.6 µm

Wavelength: µm
 (0.32 – 4.6)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n=1.5130-0.003169λ^{2}+0.003962λ^{-2}$$

Comments

Grey soda lime silica window glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. Rubin. Optical properties of soda lime silica glasses, Solar Energy Materials 12, 275-288 (1985)