Optical constants of SCHOTT - multiple purpose
ZERODUR®

Wavelength: µm
 (0.365 – 2.325)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.3182408λ^2}{λ^2-0.00879}+\frac{0.0244λ^2}{λ^2-0.0609}+\frac{1.08915181λ^2}{λ^2-110}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

SCHOTT Technical Information: Optical Properties of ZERODUR, November 2007

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.