RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - multiple purpose
D 263® T eco Thin Glass

Wavelength: µm
 (0.334 – 2.325)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.23795755λ^2}{λ^2-0.00863080926}+\frac{0.0466468888λ^2}{λ^2-0.0469074501}+\frac{2.46700556λ^2}{λ^2-264.146296}$$

Comments

Clear borosilicate glass of high chemical resistance

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
n_d: 1.523303
V_d: 54.517200
glass_status: standard
density: 2.51 g/cm3
coefficient_of_thermal_expansion_1: 7.2e-06 K-1