RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - multiple purpose
BOROFLOAT® 33

Wavelength: µm
 (0.36501 – 1.55000)  
 

Other optical constants

logX   logY   eV

Comments

Room temperature. ORIENTATION VALUES ONLY!

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Datasheet "BOROFLOAT® 33 glass - Optical Properties", SCHOTT North America Inc. (2014)
(Courtesy of SCHOTT North America)

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.