RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - multiple purpose
AF 32® eco Thin Glass

Wavelength: µm
 (0.31 – 2.325)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.11332955λ^2}{λ^2-0.00707493977}+\frac{0.141527282λ^2}{λ^2-0.0225358637}+\frac{0.860743147λ^2}{λ^2-90.1552652}$$

Comments

Alkali free alumino borosilicate glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
n_d: 1.511531
V_d: 62.574031
glass_status: standard
density: 2.43 g/cm3
coefficient_of_thermal_expansion_1: 3.2e-06 K-1

References

SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.