RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - SF (Dense flint)
SF57HTultra

Wavelength: µm
 (0.37 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.81651371λ^2}{λ^2-0.0143704198}+\frac{0.428893641λ^2}{λ^2-0.0592801172}+\frac{1.07186278λ^2}{λ^2-121.419942}$$

Comments

lead containing glass type. suitable for precision molding. step 0.5 available

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 7.26e-06 1.88e-08 -5.14e-11 1.96e-06 1.79e-09 0.276
n_d: 1.84666
V_d: 23.83
glass_code: 847238.551
glass_status: standard
density: 5.51 g/cm3
coefficient_of_thermal_expansion_1: 8.3e-06 K-1
coefficient_of_thermal_expansion_2: 9.2e-06 K-1
ΔP_gF: 0.0123
climatic_resistance: 2.0
stain_resistance: 5.0
acid_resistance: 52.3
alkali_resistance: 2.3
phosphate_resistance: 4.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links