Optical constants of SCHOTT - SF (Dense flint)
N-SF6HT

Wavelength: µm
 (0.37 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.77931763λ^2}{λ^2-0.0133714182}+\frac{0.338149866λ^2}{λ^2-0.0617533621}+\frac{2.08734474λ^2}{λ^2-174.01759}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -4.93e-06 7.02e-09 -2.4e-11 9.84e-07 1.54e-09 0.29
n_d: 1.80518
V_d: 25.36
glass_code: 805254.337
glass_status: standard
density: 3.369 g/cm3
coefficient_of_thermal_expansion_1: 9.03e-06 K-1
coefficient_of_thermal_expansion_2: 1.034e-05 K-1
ΔP_gF: 0.0146
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 2.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links