RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - SF (Dense flint)
N-SF15

Wavelength: µm
 (0.37 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.57055634λ^2}{λ^2-0.0116507014}+\frac{0.218987094λ^2}{λ^2-0.0597856897}+\frac{1.50824017λ^2}{λ^2-132.709339}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -7.15e-07 1.04e-08 -2.62e-11 8.56e-07 1.29e-09 0.281
n_d: 1.69892
V_d: 30.2
glass_code: 699302.292
glass_status: standard
density: 2.921 g/cm3
coefficient_of_thermal_expansion_1: 8.04e-06 K-1
coefficient_of_thermal_expansion_2: 9.28e-06 K-1
ΔP_gF: 0.0108
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.