Optical constants of SCHOTT - PK (Phosphate crown)
N-PK51

Wavelength: µm
 (0.3 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.15610775λ^2}{λ^2-0.00585597402}+\frac{0.153229344λ^2}{λ^2-0.0194072416}+\frac{0.785618966λ^2}{λ^2-140.537046}$$

Comments

suitable for precision molding. step 0.5 available

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -1.98e-05 -6.06e-09 1.6e-11 4.16e-07 5.01e-10 0.134
n_d: 1.52855
V_d: 76.98
glass_code: 529770.386
glass_status: standard
density: 3.855 g/cm3
coefficient_of_thermal_expansion_1: 1.235e-05 K-1
coefficient_of_thermal_expansion_2: 1.412e-05 K-1
ΔP_gF: 0.0258
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 52.3
alkali_resistance: 3.3
phosphate_resistance: 4.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22