RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - LaSF (Lanthanum dense flint)
P-LASF47

Wavelength: µm
 (0.334 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.85543101λ^2}{λ^2-0.0100328203}+\frac{0.315854649λ^2}{λ^2-0.0387095168}+\frac{1.28561839λ^2}{λ^2-94.5421507}$$

Comments

suitable for precision molding

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 7.87e-06 1.09e-08 -1.56e-11 7.58e-07 8.92e-10 0.218
n_d: 1.8061
V_d: 40.9
glass_code: 806409.454
glass_status: standard
density: 4.538 g/cm3
coefficient_of_thermal_expansion_1: 6.04e-06 K-1
coefficient_of_thermal_expansion_2: 7.27e-06 K-1
ΔP_gF: -0.0079
climatic_resistance: 1.0
stain_resistance: 1.0
acid_resistance: 51.4
alkali_resistance: 1.0
phosphate_resistance: 2.2

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.