Optical constants of SCHOTT - LaSF (Lanthanum dense flint)
N-LASF45

Wavelength: µm
 (0.365 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.87140198λ^2}{λ^2-0.011217192}+\frac{0.267777879λ^2}{λ^2-0.0505134972}+\frac{1.73030008λ^2}{λ^2-147.106505}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 2.78e-06 8.73e-09 -2.65e-11 8.24e-07 1.15e-09 0.255
n_d: 1.80107
V_d: 34.97
glass_code: 801350.363
glass_status: standard
density: 3.626 g/cm3
coefficient_of_thermal_expansion_1: 7.36e-06 K-1
coefficient_of_thermal_expansion_2: 8.56e-06 K-1
ΔP_gF: 0.0009
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 3.2
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22