Optical constants of SCHOTT - LaSF (Lanthanum dense flint)
N-LASF44

Wavelength: µm
 (0.334 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.78897105λ^2}{λ^2-0.00872506277}+\frac{0.38675867λ^2}{λ^2-0.0308085023}+\frac{1.30506243λ^2}{λ^2-92.7743824}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 3.32e-06 1.12e-08 -8.52e-12 5.88e-07 7.13e-10 0.209
n_d: 1.8042
V_d: 46.5
glass_code: 804465.444
glass_status: standard
density: 4.44 g/cm3
coefficient_of_thermal_expansion_1: 6.21e-06 K-1
coefficient_of_thermal_expansion_2: 7.39e-06 K-1
ΔP_gF: -0.0084
climatic_resistance: 1.0
stain_resistance: 1.0
acid_resistance: 4.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22