Optical constants of SCHOTT - LaSF (Lanthanum dense flint)
N-LASF31A

Wavelength: µm
 (0.334 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.96485075λ^2}{λ^2-0.00982060155}+\frac{0.475231259λ^2}{λ^2-0.0344713438}+\frac{1.48360109λ^2}{λ^2-110.739863}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.67e-06 8.9e-09 -8.73e-12 7.47e-07 7.46e-10 0.207
n_d: 1.883
V_d: 40.76
glass_code: 883408.551
glass_status: standard
density: 5.51 g/cm3
coefficient_of_thermal_expansion_1: 6.74e-06 K-1
coefficient_of_thermal_expansion_2: 7.72e-06 K-1
ΔP_gF: -0.0085
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 2.3
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.