Optical constants of SCHOTT - LaK (Lanthanum crown)
N-LAK8

Wavelength: µm
 (0.31 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.33183167λ^2}{λ^2-0.00620023871}+\frac{0.546623206λ^2}{λ^2-0.0216465439}+\frac{1.19084015λ^2}{λ^2-82.5827736}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 4.1e-06 1.25e-08 -1.6e-11 4.3e-07 6.29e-10 0.213
n_d: 1.713
V_d: 53.83
glass_code: 713538.375
glass_status: standard
density: 3.749 g/cm3
coefficient_of_thermal_expansion_1: 5.6e-06 K-1
coefficient_of_thermal_expansion_2: 6.7e-06 K-1
ΔP_gF: -0.0083
climatic_resistance: 3.0
stain_resistance: 2.0
acid_resistance: 52.3
alkali_resistance: 1.0
phosphate_resistance: 3.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.