RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - LaK (Lanthanum crown)
N-LAK34

Wavelength: µm
 (0.29 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.26661442λ^2}{λ^2-0.00589278062}+\frac{0.665919318λ^2}{λ^2-0.0197509041}+\frac{1.1249612λ^2}{λ^2-78.8894174}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.96e-06 9.65e-09 4.4e-12 4.91e-07 5.28e-10 0.161
n_d: 1.72916
V_d: 54.5
glass_code: 729545.402
glass_status: standard
density: 4.02 g/cm3
coefficient_of_thermal_expansion_1: 5.81e-06 K-1
coefficient_of_thermal_expansion_2: 6.91e-06 K-1
ΔP_gF: -0.0079
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 52.3
alkali_resistance: 1.0
phosphate_resistance: 3.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.