RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - LaK (Lanthanum crown)
N-LAK33B

Wavelength: µm
 (0.3 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.42288601λ^2}{λ^2-0.00670283452}+\frac{0.593661336λ^2}{λ^2-0.021941621}+\frac{1.1613526λ^2}{λ^2-80.7407701}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 2.77e-06 1.24e-08 1.22e-11 5.19e-07 6.02e-10 0.184
n_d: 1.755
V_d: 52.3
glass_code: 755523.422
glass_status: standard
density: 4.221 g/cm3
coefficient_of_thermal_expansion_1: 5.83e-06 K-1
coefficient_of_thermal_expansion_2: 7.06e-06 K-1
ΔP_gF: -0.0085
climatic_resistance: 1.0
stain_resistance: 1.0
acid_resistance: 51.3
alkali_resistance: 1.0
phosphate_resistance: 2.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.