RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - LaK (Lanthanum crown)
N-LAK14

Wavelength: µm
 (0.31 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.50781212λ^2}{λ^2-0.00746098727}+\frac{0.318866829λ^2}{λ^2-0.0242024834}+\frac{1.14287213λ^2}{λ^2-80.9565165}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 2.68e-06 1.15e-08 -1.44e-11 3.72e-07 5.53e-10 0.226
n_d: 1.6968
V_d: 55.41
glass_code: 697554.363
glass_status: standard
density: 3.63 g/cm3
coefficient_of_thermal_expansion_1: 5.5e-06 K-1
coefficient_of_thermal_expansion_2: 6.9e-06 K-1
ΔP_gF: -0.0079
climatic_resistance: 3.0
stain_resistance: 2.0
acid_resistance: 52.3
alkali_resistance: 1.0
phosphate_resistance: 3.0

References

1) SCHOTT optical glass data sheets 2015-07-22