RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - LaK (Lanthanum crown)
N-LAK10

Wavelength: µm
 (0.35 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.72878017λ^2}{λ^2-0.00886014635}+\frac{0.169257825λ^2}{λ^2-0.0363416509}+\frac{1.19386956λ^2}{λ^2-82.9009069}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 4.1e-06 1.23e-08 -7.85e-12 5.08e-07 5.76e-10 0.205
n_d: 1.72003
V_d: 50.62
glass_code: 720506.369
glass_status: standard
density: 3.689 g/cm3
coefficient_of_thermal_expansion_1: 5.68e-06 K-1
coefficient_of_thermal_expansion_2: 6.83e-06 K-1
ΔP_gF: -0.0072
climatic_resistance: 2.0
stain_resistance: 2.0
acid_resistance: 52.3
alkali_resistance: 1.0
phosphate_resistance: 3.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki