RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - K (Crown)
K7

Wavelength: µm
 (0.31 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.1273555λ^2}{λ^2-0.00720341707}+\frac{0.124412303λ^2}{λ^2-0.0269835916}+\frac{0.827100531λ^2}{λ^2-100.384588}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -1.67e-06 8.8e-09 -2.86e-11 5.42e-07 7.81e-10 0.172
n_d: 1.51112
V_d: 60.41
glass_code: 511604.253
glass_status: standard
density: 2.53 g/cm3
coefficient_of_thermal_expansion_1: 8.4e-06 K-1
coefficient_of_thermal_expansion_2: 9.7e-06 K-1
climatic_resistance: 3.0
stain_resistance: 0.0
acid_resistance: 2.0
alkali_resistance: 1.0
phosphate_resistance: 2.3

References

1) SCHOTT optical glass data sheets 2015-07-22