RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - BaSF (Barium dense flint)
N-BASF2

Wavelength: µm
 (0.37 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.53652081λ^2}{λ^2-0.0108435729}+\frac{0.156971102λ^2}{λ^2-0.0562278762}+\frac{1.30196815λ^2}{λ^2-131.3397}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.89e-06 1.22e-08 -1.61e-11 7.77e-07 9.96e-10 0.256
n_d: 1.66446
V_d: 36
glass_code: 664360.315
glass_status: standard
density: 3.151 g/cm3
coefficient_of_thermal_expansion_1: 7.12e-06 K-1
coefficient_of_thermal_expansion_2: 8.13e-06 K-1
ΔP_gF: 0.0057
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.