Optical constants of SCHOTT - BaLF (Barium light flint)
N-BALF5

Wavelength: µm
 (0.35 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.28385965λ^2}{λ^2-0.00825815975}+\frac{0.0719300942λ^2}{λ^2-0.0441920027}+\frac{1.05048927λ^2}{λ^2-107.097324}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.14e-06 1.29e-08 -1.46e-11 5.02e-07 5.87e-10 0.219
n_d: 1.54739
V_d: 53.63
glass_code: 547536.261
glass_status: standard
density: 2.614 g/cm3
coefficient_of_thermal_expansion_1: 7.34e-06 K-1
coefficient_of_thermal_expansion_2: 8.43e-06 K-1
ΔP_gF: -0.0004
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 2.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links