RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - BaLF (Barium light flint)
N-BALF4

Wavelength: µm
 (0.35 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.31004128λ^2}{λ^2-0.0079659645}+\frac{0.142038259λ^2}{λ^2-0.0330672072}+\frac{0.964929351λ^2}{λ^2-109.19732}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 5.33e-06 1.47e-08 -1.58e-11 5.75e-07 6.58e-10 0.195
n_d: 1.57956
V_d: 53.87
glass_code: 580539.311
glass_status: standard
density: 3.111 g/cm3
coefficient_of_thermal_expansion_1: 6.52e-06 K-1
coefficient_of_thermal_expansion_2: 7.41e-06 K-1
ΔP_gF: -0.0012
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links