RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of HIKARI - Glasses for precision molding
Q-LASFH59S

Wavelength: µm
 (0.320 – 2.400)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula

$$n^2=3.22581362-0.0128335027λ^{2}-9.26420505\text{×}10^{-05}λ^{4}+0.0304553203λ^{-2}+0.000747766899λ^{-4}-1.21365984\text{×}10^{-06}λ^{-6}+1.90023535\text{×}10^{-06}λ^{-8}$$

Comments

For mold lens

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 23.0 °C
n_d: 1.820980
V_d: 42.502165
density: 4.81 g/cm3
coefficient_of_thermal_expansion_1: 6e-06 K-1
ΔP_gF: -0.0081
phosphate_resistance: 1.0

References

1) HIKARI optical glass catalog 2015-04-01
2) HIKARI Zemax catalog

More info - wiki

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.

External links

Latest optical glass catalog