Optical constants of HIKARI - Glasses for precision molding
Q-LASFH58S

Wavelength: µm
 (0.330 – 2.400)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula

$$n^2=3.32552726-0.0132706113λ^{2}-0.000149120991λ^{4}+0.0339899628λ^{-2}+0.000811209445λ^{-4}+5.79662969\text{×}10^{-06}λ^{-6}+2.35145894\text{×}10^{-06}λ^{-8}$$

Comments

For mold lens

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 23.0 °C
n_d: 1.851080
V_d: 40.123706
density: 5.03 g/cm3
coefficient_of_thermal_expansion_1: 6.1e-06 K-1
ΔP_gF: -0.0085
phosphate_resistance: 1.0