RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of FK51A
N-FK51A (SCHOTT)

Wavelength: µm
 (0.29 – 2.5)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.971247817λ^2}{λ^2-0.00472301995}+\frac{0.216901417λ^2}{λ^2-0.0153575612}+\frac{0.904651666λ^2}{λ^2-168.68133}$$

Comments

suitable for precision molding. step 0.5 available

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -1.83e-05 -7.89e-09 -1.63e-12 3.74e-07 3.46e-10 0.15
n_d: 1.48656
V_d: 84.47
glass_code: 487845.368
glass_status: standard
density: 3.675 g/cm3
coefficient_of_thermal_expansion_1: 1.274e-05 K-1
coefficient_of_thermal_expansion_2: 1.481e-05 K-1
ΔP_gF: 0.0342
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 52.3
alkali_resistance: 2.2
phosphate_resistance: 4.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

N-FK51A is a popular optical glass produced by Schott AG