Optical constants of CDGM - ZK (Dense crown)
H-ZK1

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.4273402-1.0813896\text{×}10^{-2}λ^{2}+1.2437975\text{×}10^{-2}λ^{-2}+2.2593135\text{×}10^{-4}λ^{-4}-7.6715617\text{×}10^{-6}λ^{-6}+6.5496402\text{×}10^{-7}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]