Optical constants of CDGM - ZF (Dense flint)
ZF11

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.7906689-1.0644977\text{×}10^{-2}λ^{2}+2.9071854\text{×}10^{-2}λ^{-2}+2.1286607\text{×}10^{-3}λ^{-4}-1.5815625\text{×}10^{-4}λ^{-6}+1.7145247\text{×}10^{-5}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database