Optical constants of CDGM - QF (Light flint)
QF6

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.3044884-8.3782321\text{×}10^{-3}λ^{2}+1.4424342\text{×}10^{-2}λ^{-2}+3.3374311\text{×}10^{-4}λ^{-4}-4.4657456\text{×}10^{-6}λ^{-6}+1.3349929\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers